How to print tooth brush silicone effect on elastic? taps

Printing tips for silicone tooth brush effect printing Preparation: Mesh&Squeegee: HD and glossy screen Mesh number 120-150 (48-59T),CMYK Mesh number300(120T)   ; Squeegee 65-75 degree Squeegee sharp and flat. Pigments added ratio:For white and fluorescent color 20%,other color 10% Catalyst mixing ratio:10% Silicone thinner XG-128AH adding ratio:10-30% ,brush printing need more silicone thinner. Heating Temp and time: Flash cure temp :80℃-100℃ for 6-10 seconds ,after finish printing to...

How to print CMYK silicone & glossy silicone effect on elastic taps?

Printing tips for silicone CMYK glossy silicone effect printing Preparation: Mesh&Squeegee: HD and glossy screen Mesh number 120-150 (48-59T), CMYK Mesh number300(120T) ;Squeegee 65-75 degrees Squeegee sharp and flat.Pigments added ratio: For white and fluorescent colors 20%, other colors 10%Catalyst mixing ratio:10%Silicone thinner XG-128AH adding ratio:10-20% :20% Heating Temp and time: Flash cure temp:100℃- 120℃ for 6-10 seconds, after finish printing to...

How to print Elastic Webbing by golden glossy silicone effect?

Printing Tips HD Golden Glossy Silicone Ink for Ribbons printing Preparation: Mesh&Squeegee: 120(48T) Mesh number ;Squeegee 65-75 degrees Squeegee sharp and flat.Pigments added ratio: For white and fluorescent colors 20%, other colors 10%Catalyst mixing ratio:10%Silicone thinner XG-128AH adding ratio:10-20% :20%Heating Temp and time: Flash cure temp:100℃- 120℃ for 6-10 seconds, after finish printing to dry by temp:120℃- 140℃ for about...

How to print matte dotting silicone effect on HD matte silicone printing?

HD matte silicone ink printing process: Preparation: Mesh&Squeegee: 120(48T) Mesh number; 65-75 degree Squeegee.: Pigments added ratio:For white and fluorescent color 20%,other color 10%Catalyst mixing ratio:2% Silicone thinner XG-128AH adding ratio:0-20%    Heating Temp and time: Flash cure temp :100℃- 120℃ for 6-10 seconds, Drying temp :120℃ for about 2 -3 minutes. 1.Screen printing silicone print 3 layers: Screen Printing silicone  XG-866A-2Y  100G Silicone catalyst              XG-866B-2     2G   2% Silicone thinner              XG-128AH   20G  20% Flash temp...

How to print HD super soft matte silicone effect?

Tips printing process for soft matte effect printing Preparation: Mesh&Squeegee: 120(48T) Mesh number; 65-75 degree Squeegee.: Pigments added ratio: For white and fluorescent colors 20%, other colors 10%Catalyst mixing ratio:2% Silicone thinner XG-128A adding ratio:0-20%    Heating Temp and time: Flash cure temp: 100℃- 120℃ for 6-10 seconds, Drying temp: 120℃- 140℃ for about 2 -3 minutes. Silicone ink printing tips: 1. HD silicone XG-866A/866AH for under coating  and high density printing for...

How to Screen Print HD glossy golden silicone Effect?

Tips for golden silicone ink printing Preparation: Mesh&Squeegee: 120(48T) Mesh number; 65-75 degree Squeegee.Pigments added ratio: For white and fluorescent colors 20%, other colors 10%, glitter powders 10%.Catalyst mixing ratio: 2% slow dry XG-866B-1 and fast dry XG-866B-2 can mix together for use.Silicone thinner XG-128A adding ratio: 0-20% Silicone thinner is not necessary for hand printingHeating Temp and time: Flash cure temp:100℃- 120℃ for 6-10 seconds, Drying temp: 120℃- 140℃ for 2-3...

How to print supper smooth glossy silicone effect?

Key points for HD Glossy Silicone Ink Screen Printing 1st To make a thick screen  2nd For the hairy fabric, to heat press by heat press machine or iron after first-time silicone printing for smooth effect. Silicone ink is sticky when lifting up the screen and heated all fabric hairy will stand up, if heat presses then all fabric hairy will lie flat...

How to 3D Emboss Silicone Screen Printing for Sportswear fabric?

Mesh number 80-120 (32-48T) Embossing printing silicone ink and catalyst Mixing Ratio: Embossing silicone ink  XG-360KY-55:  50G Embossing silicone catalyst XG-360BH:   5G   (mixing ratio 10%) Silicone thinner  XG-128AH: not necessary Print mixing silicone ink on the backside of the fabric Machine temp set temp : Upper mold 180 degree Bottom mold 120-150 degree Can stick a thin fabric on the printing fabric backside   (depends on  design ) Heating time 8-15 seconds   (depends...

How to print anti-slip silicone ink on a gloves printing machine?

Anti-slip gloves printing silicone ink printing tips: Preparation: Mesh: 30-60(12T-24T) to make a thick screen by emulsion. Better to use Hollow aluminum.Pigments added ratio:2-4%Catalyst mixing ratio:2% Thinner XG-128AH adding ratio:0-10%    thinner is not necessary Heating Temp and time: 120℃ -150℃ for 6-12 seconds, Heating time depends on drying temp. Silicone ink mixing tips: Printing silicone       XG-15A        60G Catalyst               XG-15B       1.2G  (2%) Pigment              XG-           1.2-2.4G  (2-4%) If need color effect To print by thick...

How to dip soft taps for a good sharp and supper soft smooth matte silicone effect?

Dipping tips for hard hand feel and dipping silicone ink and soft smooth dipping silicone ink: 1st  Dip hard hand feel silicone Clear layer 1 time The Hard hand feel silicone        XG-60S   100G The Hard hand feel silicone catalyst  XG-60S-ZB    10G  10% (10G silicone to mix with 1G catalyst) No need to mix with silicone thinner To dip one time and wait about 40-70 minutes...