How to Print Suede Socks Printing Silicone Ink?

Suede Socks Printing Silicone Ink: XG-15T+ &catalyst XG-15B Preparation: Mesh: 30-60(12T-24T) to make a thick screen by emulsion.Can use Hollow aluminum screen.Pigments added ratio:4%Catalyst mixing ratio:2% Thinner XG-128AH adding ratio:0-10% thinner is not necessary Heating Temp and time: 150℃ -170℃ for 6-12 seconds, Heating time depends on drying temp. Silicone ink mixing tips: Printing silicone       XG-15T        50G Catalyst               XG-15B+       1 G  (2%) Pigment              XG-            2G  (4%) Silicone ink mixing tips: Print two strokes by one layer. To print by...

Screen Printing Silicone Ink for Printing Anti-Slip Socks

Preparation: Mesh: 30-60(12T-24T) to make a thick screen by emulsion. Better to use Hollow aluminum.Pigments added ratio:2-4%Catalyst mixing ratio:2% Thinner XG-128AH adding ratio:0-10% thinner is not necessary Heating Temp and time: 120℃ -150℃ for 6-12 seconds, Heating time depends on drying temp. Silicone ink mixing tips: Printing silicone       XG-15A+        60G Catalyst               XG-15B+       1.2G  (2%) Pigment              XG-           1.2-2.4G  (2-4%) If need color effect To print by thick screen and big holes mesh for...

Anti Slip Socks Silicone Ink Printing

Anti slip socks silicone ink XG-15A &catalyst XG-15B   Preparation: 1.Mesh: 30-60(12T-24T) to make thick screen by emulsion. 2.Pigments added ratio:2-4% 3.Catalyst mixing ratio:2%  4.Thinner XG-128AH adding ratio:0-10%    thinner is not necessary 5.Heating Temp and time: 120℃ -150℃ for 6-12 seconds , Heating time depends on drying temp.   Silicone ink mixing tips: Socks silicone       XG-15A       60G Catalyst              XG-15B      1.2G (2%) Thinner              XG-128AH    0-6G (0-10%) Pigment             XG-          1.2-2.4G (2-4%) If need color effect To print by thick screen...

Hello~