Suede Socks Printing Silicone Ink: XG-15T+ &catalyst XG-15B

Preparation:

  1. Mesh: 30-60(12T-24T) to make a thick screen by emulsion.Can use Hollow aluminum screen.
  2. Pigments added ratio:4%
  3. Catalyst mixing ratio:2%
  4. Thinner XG-128AH adding ratio:0-10% thinner is not necessary
  5. Heating Temp and time: 150℃ -170℃ for 6-12 seconds, Heating time depends on drying temp.

Silicone ink mixing tips:

Printing silicone       XG-15T        50G

Catalyst               XG-15B+       1 G  (2%)

Pigment              XG-            2G  (4%)

Silicone ink mixing tips:

Print two strokes by one layer.

To print by thick screen and big holes mesh for one layer then finish and heating by 150℃ -170℃ for 6-12 seconds, Heating time depends on drying temp.

Socks Printing Suede Silicone ink Dotting, Anti-Slip Suede Silicone for socks
Socks Printing Suede Silicone ink Dotting Anti-Slip Suede Silicone for socks

Share this post

0 0 votes
Article Rating
Subscribe
Notify of
guest
0 评论
Inline Feedbacks
View all comments

Hello~

0
Would love your thoughts, please comment.x
()
x