If dark color fabric print CMYK effect need to print a full screen printing white color for 1-2 times first then print CMYK effect.
If fabric with hairy have to print a full screen printing for under printing two times ,for first time printing assist by heat press machine or iron after first time printing to get good smooth. After printing keep wet to heat press by temp 150-170 degree for 10-20 seconds.Second printing same as normal silicone printing heat by 120℃- 140℃ for 6-10 seconds.
After finish to heat by heating tunnel by 120-140 degree for 2 -3 minutes