Dipping Silicone ink for Sholace Tipping

Silicone ink for Shoelace tipping /shoelace dipping process TDS of XG shoelace dipping silicone 1st  Dipping silicone Clear layer 1 time Dipping silicone XG-20S    100G Fast dry catalyst  XG-KB    10G  10% (10G silicone to mix with 1G catalyst) Thinner XG-128AH         100-120G   100-120%  (10G silicone to mix with 10-12G thinner) To dip one time and wait about 40-70 minutes to get...

Silicone Transfer by Hotmelt Powder

silicone transfer stickers by hot melt powder Silicone ink PET films: Two types : one is glossy coating film which will be glossy after heating press on fabric ,another one is matte finish effect after heating press on fabric. Mesh number: 120-200 , Mesh(screen film )thickness 0.1-0.2MM,it is depends on printing Artworks. Squeegee:65-80 degree . Printing tips: 1 Silicone ink color layer printing for 3-4 layers  : Silicone...

Silicone Transfer by Glue

silicone transfer stickers by glue Silicone ink PET films: Two types : one is glossy coating film which will be glossy after heating press on fabric ,another one is matte finish effect after heating press on fabric. Mesh number: 120-200 , Mesh(screen film )thickness 0.1-0.2MM,it is depends on printing Artworks. Squeegee:65-80 degree . Printing tips: 1 Silicone ink color layer printing for 3-4 layers Silicone ink     XG-866A-2Y       100G Pigments or...

Silicone Brush Transfer Sticker Logos Making

Tags: Silicone brush stickers, brush silicone transfer logos, brush logos making Silicone ink PET films: To choose matte coating PET films Mesh number: 120-200 , Mesh(screen film )thickness 0.1-0.2MM,it is depends on printing Artworks. Squeegee:65-80 degree . 1 Printing tips:Hot melt glue XG-360R-2X print for 4-6 times When printing glue to use cyclohexanone to liquid the glue,mixing ratio 10%.This type of glue easy to be thick and mesh printing.   Flash by room temp or by 100-120 degree. 2...

Embossing Silicone

T-shirt/fabric/silicone ink Embossing process, silicone ink for silicone embossing machine, 3D Embossing silicone ink for fabric embossing machine process Code number: XG-360KY-55 &catalyst XG-360BH XG-360KY-65&catalyst XG-360BH1 Mesh number 80-120 (32-48T) 1st Embossing silicone ink mixing: Embossing silicone ink  XG-360KY-55/XG-360KY-65 :  50G Embossing silicone catalyst XG-360BH/XG-360BH1:   5G   (mixing ratio 10%) Silicone thinner : not necessary 2nd Printing mixing silicone...

HD Glossy Silicone Transfers Sticker Logo Making

Tags: HD glossy silicone transfers,  HD transfer stickers Silicone logo, Transfer logo,transfer silicone, silicone transfer stickers making Silicone ink PET films: To choose matte coating PET films Mesh number: 120-200 , Mesh(screen film )thickness 0.1-0.2MM,it is depends on printing Artworks. Squeegee:65-80 degree . Printing tips: 1 Hot melt glue XG-360R-3 print for 4-6 times When printing glue to use cyclohexanone to liquid the glue,mixing ratio 10%.This type of glue easy...

Mould Pressing Silicone Transfer Stickers Making

XG-360W & catalyst XG-360WB Silicone transfer stickers making by mould and hot melt paper,moulding silicone transfer stickers,transfer logos by mould press making process: 1st : Filling bellow mixing moulding silicone ink together into the mould Moulding silicone XG-360W 60G Silicone catalyst XG-360WB 6G 10%     Pigments 1-4% 2nd: Put the hot melt paper on the silicone ink filled mould 3rd. Machine heat press ,this including vacuum , venting...

Silicone Brush Effect Printing

T-shirt/fabric/silicone ink brush printing and silicone high density brush dots printing Preparation: Mesh&Squeegee: 120(48T) Mesh number ;65-75 degree Squeegee.: Pigments added ratio:For white and fluorescent color 20%,other color 10%Catalyst mixing ratio:2% slow dry XG-866B-1 and fast dry XG-866B-2 can mix together for using.Thinner XG-128A adding ratio:10-30%    thinner is very necessary for brush printing Heating Temp and time: Flash cure temp :100℃- 120℃ for...

Anti Slip Socks Silicone Ink Printing

Anti slip socks silicone ink XG-15A &catalyst XG-15B   Preparation: 1.Mesh: 30-60(12T-24T) to make thick screen by emulsion. 2.Pigments added ratio:2-4% 3.Catalyst mixing ratio:2%  4.Thinner XG-128AH adding ratio:0-10%    thinner is not necessary 5.Heating Temp and time: 120℃ -150℃ for 6-12 seconds , Heating time depends on drying temp.   Silicone ink mixing tips: Socks silicone       XG-15A       60G Catalyst              XG-15B      1.2G (2%) Thinner              XG-128AH    0-6G (0-10%) Pigment             XG-          1.2-2.4G (2-4%) If need color effect To print by thick screen...

Moulding Silicone Ink

XG-360W & catalyst XG-360WB 1st Mixing moulding silicone ink Moulding silicone ink XG-360W           50G Moulding silicone catalyst XG-360WB        5G   (mixing ratio 10%) Silicone thinner   : 0-10% Silicone pigments  2-4% 2nd Vacuum by vacuum machine Mixing together well and vacuum by vacuum machine.  Fill the liquid moulding silicone on the mold move to vacuum by vacuum machine 3rd Fill the vacuumed silicone ink on the...