Anti slip socks silicone ink

XG-15A &catalyst XG-15B
 
Preparation:
1.Mesh: 30-60(12T-24T) to make thick screen by emulsion.
2.Pigments added ratio:2-4%
3.Catalyst mixing ratio:2% 
4.Thinner XG-128AH adding ratio:0-10%    thinner is not necessary
5.Heating Temp and time: 120℃ -150℃ for 6-12 seconds , Heating time depends on drying temp.
 
Silicone ink mixing tips:
Socks silicone       XG-15A       60G
Catalyst              XG-15B      1.2G (2%)
Thinner              XG-128AH    0-6G (0-10%)
Pigment             XG-          1.2-2.4G (2-4%) If need color effect

To print by thick screen and big holes mesh for one layer then finish and heating by 120℃ -150℃ for 6-12 seconds , Heating time depends on drying temp.

XG anti-slip silicone machine printing silicone
XG silicone for socks printing machine
XG silicone gloves dotting silicone anti-slip silicone
Anti slip socks silicone ink printing
Anti slip socks silicone ink printing
Anti slip socks silicone ink printing
Anti slip socks silicone ink printing

Share this post

3 2 votes
Article Rating
Subscribe
Notify of
guest
0 评论
Inline Feedbacks
View all comments

Hello~

0
Would love your thoughts, please comment.x
()
x